I've done this before, but after I sanded them down to 'full foggy', I then began the 'repolishing'.... Many stages from 400 back up to 2400 grit. Then 3 steps of super fine liquid polish
This process seems to be a stong solvent to convert the rough-but-uniform surface into a liquid which then 'flows' and re-cures into a smooth surface....
|